FEATURES
-
Excellent Resistance to severe fine
Abrasion under Low to Moderate Impact at
both Ambient and elevated temperature
upto 800 Deg. C.
-
Weld-Metal recovery is as high as 80 to
85 %.
-
High Deposition rate, No slag removal,
Non-hygroscopic coating and No
pre-drying.
-
Longer shelf-life.
TYPICAL
APPLICATIONS : Sinter breakers, sinter
fans, clinker wear parts, blast furnace
bells & hoppers etc. ALLOY BASIS
: C. Cr, Mo, Nb, W, V
STRUCTURE
: Weld-metal contains Complex Carbides of
Cr, Mo, Nb, W in tough Austenitic Matrix.
HARDNESS : Two Layers 62 to 65 Rc.
RECOMMENDED CURRENT
: DC (+) Preferred / AC 70 OCV
|
Size (mm)
|
Amps
|
|
6.30 x 450
|
75 to 130
|
|
8.00 x 450 |
110 to 160 |
|
10.00 x 450 |
130 to 180 |
IDENTIFICATION
: Tip Color - POST OFFICE RED
Surface Relief-Checks in weld-metal are
normal and infact, desirable. These checks
prevent stress build-up because of high
hardness and high-alloy contents. |